Filler metal A showed 50% of its grain boundary area cracked, while filler metal B had 90% of its fusion zone grain boundaries cracked, evinced by the presence of 10-500-μm cracks on the grain ...
Chromium-molybdenum (chrome-moly) pipe has become a standard in the power generation industry, not only because of its corrosion resistance and high-temperature strength, but also for its ...
Brazing joins parts by heating them to more than 840°F and applying a filler metal that has a melting temperature below that of the base metal. Filler metal flows into the joint by capillary ...
Addman Advanced Metals has scaled from a single 3D printer to 25 while also building out a robust array of subtractive machines. In this video, find out how the shop manages its additive and ...